[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1274162":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1274162,860,2,"多选题","内墙和顶棚涂料涂层色淡易掉粉的原因分析包括（ ）。",[11,15,18,22,25],{"key":12,"text":13,"correct":14},"A","控制好骨料稠度，专人负责搅拌",false,{"key":16,"text":17,"correct":14},"B","基层应干湿一致",{"key":19,"text":20,"correct":21},"C","使用涂料时未搅拌均匀",true,{"key":23,"text":24,"correct":21},"D","涂料质量不合标准，耐水性能不合格",{"key":26,"text":27,"correct":14},"E","停歇前，应有专人作好未成活部位的遮挡工作，若已溅上骨料应及时清除","CD","内墙和顶棚涂料涂层色淡易掉粉的原因分析：①使用涂料时未搅拌均匀。桶内上部料稀，色料上浮，遮盖力差；下面料稠，填料沉淀，色淡，涂刷后易脱粉。②涂料质量不合标准，耐水性能不合格。③混凝土及砂浆基层龄期短，含水率高，碱度大。④施工涂刷时，气温低于涂料最低成膜温度，或涂料未成膜即被水冲洗。⑤涂料加水过多，涂料太稀，成膜不完善。",{"id":6,"name":31,"category":32,"favorite":33},"(装饰质量)专业管理实务 岗位知识","建筑工程",0]