[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1268869":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":19,"analysis":25},1268869,856,1,"单选题","水泥混凝土桥面铺装层的裂纹和龟裂原因不包括（ ）",[11,15,18,22],{"key":12,"text":13,"correct":14},"A","砂石原材料质量不合格",false,{"key":16,"text":17,"correct":14},"B","水泥混凝土铺装层与梁板结构未能很好地连接成为整体，有“空鼓”现象",{"key":19,"text":20,"correct":21},"C","桥面铺装层内钢筋网上保护层偏小，钢筋网未能起到防裂作用",true,{"key":23,"text":24,"correct":14},"D","未按施工方案要求进行养护及封闭施工，桥面铺筑完成后养护不及时，在混凝土尚未达到设计强度时即开放交通，造成了铺装的早期破坏","水泥混凝土桥面铺装层的裂纹和龟裂原因：砂石原材料质量不合格；水泥混凝土铺装层与梁板结构未能很好地连接成为整体，有“空鼓”现象；未按施工方案要求进行养护及封闭施工，桥面铺筑完成后养护不及时，在混凝土尚未达到设计强度时即开放交通，造成了铺装的早期破坏",{"id":6,"name":27,"category":28,"favorite":29},"(市政质量)专业管理实务 岗位知识","建筑工程",0]