[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1268778":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},1268778,856,1,"单选题","成卷卷材应卷紧卷齐，端面里进外出不得超过（ ）mm。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","10",true,{"key":16,"text":17,"correct":18},"B","20",false,{"key":20,"text":21,"correct":18},"C","30",{"key":23,"text":24,"correct":18},"D","40","（3）外观1）成卷卷材应卷紧、卷齐，端面里进外出不得超过10mm。2）成卷卷材在4?60°C任一产品温度下展开，在距卷芯1000mm长度外不应有10mm以上的裂纹或粘结。3）胎基应浸透，不应有未被浸渍的条纹。4）卷材表面必须平整，不允许有孔洞、缺边和裂口，矿物粒（片）料粒度应均勻一致并紧密地粘附于卷材表面。5）每卷接头处不应超过1个，较短的一段不应小于1000mm,接头应剪切整齐，并加长150mm。6）将卷材立放于平面上。用一把钢板尺平放在卷材的端面上，用另一把最小分度值为1mm的钢板尺垂直伸入卷材端面最凹处，测得的数值即为卷材端面的里进外出值。然后将卷材展开按外观质量要求检查。沿宽度方向裁取50mm宽的一条，胎基内不应有未被浸透的条纹。",{"id":6,"name":27,"category":28,"favorite":29},"(市政质量)专业管理实务 岗位知识","建筑工程",0]