[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1268698":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},1268698,856,1,"单选题","承台混凝土浇筑后，应检查承台表面无孔洞、露筋、缺棱掉角、蜂窝、麻面和宽度超过（ ）mm的收缩裂缝。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","0.1",false,{"key":16,"text":17,"correct":18},"B","0.15",true,{"key":20,"text":21,"correct":14},"C","0.2",{"key":23,"text":24,"correct":14},"D","0.25","承台混凝土浇筑后，应检查承台表面无孔洞、露筋、缺棱掉角、蜂窝、麻面和宽度超过0.15mm的收缩裂缝。",{"id":6,"name":27,"category":28,"favorite":29},"(市政质量)专业管理实务 岗位知识","建筑工程",0]