[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1267331":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},1267331,855,1,"单选题","一组电弧焊钢筋焊接接头初验试件，拉伸试验结果为：3个试件抗拉强度均大于钢筋母材的标准值，其中3个试件在焊缝处脆断，则该批接头抗拉伸性能为。（ ）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","合格",false,{"key":16,"text":17,"correct":18},"B","需复检",true,{"key":20,"text":21,"correct":14},"C","不合格",{"key":23,"text":24,"correct":14},"D","结果无效","符合下列条件之一，评定为复验。①2个试件断于钢筋母材，延性断裂，抗拉强度大于等于钢筋母材抗拉强度标准值；1个试件断于焊缝，或热影响区，呈脆性断裂，或延性断裂，抗拉强度小于钢筋母材抗拉强度标准值。②1个试件断于钢筋母材，延性断裂，抗拉强度大于等于钢筋母材抗拉强度标准值；2个试件断于焊缝，或热影响区，呈脆性断裂，抗拉强度大于等于钢筋母材抗拉强度标准值。③3个试件全部断于焊缝，或热影响区，呈脆性断裂，抗拉强度均大于等于钢筋母材抗拉强度标准值。",{"id":6,"name":27,"category":28,"favorite":29},"(市政质量)基础知识","建筑工程",0]