[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1267300":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},1267300,855,1,"单选题","普通混凝土抗压试验试件的标准养护条件是（ ）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","温度20±2℃，相对湿度为95%以上",true,{"key":16,"text":17,"correct":18},"B","温度20±5℃，相对湿度为90%以上",false,{"key":20,"text":21,"correct":18},"C","温度20±2℃，相对湿度为90%以上",{"key":23,"text":24,"correct":18},"D","温度20±1℃，相对湿度为95%以上","2）混凝土轴心抗压强度在实际工程中，混凝士结构构件大部分是棱柱体或圆柱体。为了能更好地反映混凝士的实际抗压性能，在计算钢筋混凝士构件承载力时，常采用混凝土的轴心抗压强度作为设计依据。混凝土的轴心抗压强度是采用150mmX150mmX300mm的棱柱体作为标准试件，在温度为20°C士5C环境中静置--昼夜至二昼夜后拆模，然后在标准温度条件（温度为20C士2C，相对湿度为95%以上）下养护28d至龄期，采用标准试验方法测得的抗压强度值。",{"id":6,"name":27,"category":28,"favorite":29},"(市政质量)基础知识","建筑工程",0]