[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1151321":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1151321,803,2,"多选题","（2017年）大体积混凝土施工中降低混凝土的发热量的措施有（ ）",[11,15,19,22,25],{"key":12,"text":13,"correct":14},"A","骨料预冷",false,{"key":16,"text":17,"correct":18},"B","采用低流态干硬性贫混凝土",true,{"key":20,"text":21,"correct":18},"C","增大骨料粒径",{"key":23,"text":24,"correct":18},"D","大量掺粉煤灰",{"key":26,"text":27,"correct":18},"E","采用高效减水剂","BCDE","",{"id":6,"name":31,"category":32,"favorite":33},"一建水利水电工程实务","建筑工程",0]