[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1144662":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1144662,800,2,"多选题","关于地下防水混凝土施工技术要求，正确的有（ ）。",[11,15,18,21,24],{"key":12,"text":13,"correct":14},"A","防水混凝土拌合物应采用机械搅拌，搅拌时间不小于2min",true,{"key":16,"text":17,"correct":14},"B","防水混凝土拌合物在运输后如出现离析，必须进行二次搅拌",{"key":19,"text":20,"correct":14},"C","防水混凝土应连续浇筑，宜少留施工缝",{"key":22,"text":23,"correct":14},"D","防水混凝土终凝后应立即进行养护",{"key":25,"text":26,"correct":27},"E","防水混凝土结构内部的各种钢筋和绑扎钢丝，可接触模板",false,"ABCD","2020教材P133 \u002F 2019教材P132 （4）防水混凝土拌合物应采用机械搅拌，搅拌时间不宜小于2min。 （5）防水混凝土应分层连续浇筑，分层厚度不得大于500mm并应采用机械振捣，避免漏振、欠振和超振。 （6）防水混凝土应连续浇筑，宜少留施工缝。 （8）大体积防水混凝土宜选用水化热低和凝结时间长的水泥，宜掺入减水剂、缓凝剂等外加剂和粉煤灰、磨细矿渣粉等掺合料。在设计许可的情况下，掺粉煤灰混凝土设计强度等级的龄期宜为60d或90d高温期施工时，入模温度不应大于30℃混凝土内部预埋管道，进行水冷散热。大体积防水混凝土应采取保温保湿养护，混凝土中心温度与表面温度的差值不应大于25℃，表面温度与大气温度的差值不应大于20℃，养护时间不得少于14d。",{"id":6,"name":31,"category":32,"favorite":33},"一建建筑工程实务","建筑工程",0]