[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1144661":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":19,"analysis":25},1144661,800,1,"单选题","关于地下工程防水混凝土配合比的说法，正确的是（ ）。",[11,15,18,22],{"key":12,"text":13,"correct":14},"A","水泥用量必须大于300kg\u002Fm3",false,{"key":16,"text":17,"correct":14},"B","水胶比不得大于0.45",{"key":19,"text":20,"correct":21},"C","泵送时入泵坍落度宜为120～160mm",true,{"key":23,"text":24,"correct":14},"D","预拌混凝土的初凝时间为4.5～10h","2020教材P133 \u002F 2019教材P132 （3） 防水混凝土胶凝材料总用量不宜小于320kg\u002Fm3, 在满足混凝土抗渗等级、强度等级和耐久性条件下，水泥用量不宜小于260kg\u002Fm3; 砂率宜为35% ~ 40%, 泵送时可增至45%; 水胶比不得大于0.50, 有侵蚀性介质时水胶比不宜大于0.45; 防水混凝土宜采用预拌商品混凝土，其入泵坍落度宜控制在120 ~ 160mm, 坍落度每小时损失值不应大于 20mm，总损失值不应大于40mm; 掺引气剂或引气型减水剂时，混凝土含气量应控制在 3% ~ 5%; 预拌混凝土的初凝时间宜为6 ~ 8h。",{"id":6,"name":27,"category":28,"favorite":29},"一建建筑工程实务","建筑工程",0]