[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1144452":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1144452,800,2,"多选题","下列施工措施中，有利于大体积混凝土裂缝控制的是（ ）。",[11,15,19,22,25],{"key":12,"text":13,"correct":14},"A","选用低水化热的水泥",true,{"key":16,"text":17,"correct":18},"B","提高水灰比",false,{"key":20,"text":21,"correct":18},"C","提高混凝土的入模温度",{"key":23,"text":24,"correct":14},"D","及时对混凝土进行保温、保湿养护",{"key":26,"text":27,"correct":14},"E","采用二次抹面工艺","ADE","2020版教材P101 大体积混凝土裂缝控制的主要方法之一就是降低混凝土内外温差，分降低混凝土内部温度与提高表面温度两种。A选项，选用低水化热的水泥可降低混凝土内部温度；B选项的提高水灰比有两个途径，增大用水量或者减少水泥用量。调整水灰比的前提是要满足强度、耐久、抗渗、稳定等要求，水灰比是不能随便调整改变的。为了控制裂缝降低强度就得不偿失了。C选项，提高混凝土入模温度，提高了混凝土的初始温度，增大了混凝土的内部温度。D选项，及时对混凝土进行保温、保湿养护，有助于提高混凝土的表面温度；E选项，通过二次抹面工艺，减少表面收缩裂缝。",{"id":6,"name":31,"category":32,"favorite":33},"一建建筑工程实务","建筑工程",0]