[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1144195":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1144195,800,2,"多选题","关于砌体结构砌筑用砂浆试块及其养护、抗压强度试验的说法，正确的有（ ）。",[11,15,19,22,25],{"key":12,"text":13,"correct":14},"A","立方体试块的规格尺寸为100mm×100mm×100mm",false,{"key":16,"text":17,"correct":18},"B","养护28天",true,{"key":20,"text":21,"correct":14},"C","养护相对湿度＞85%",{"key":23,"text":24,"correct":18},"D","养护温度（20±2）0C",{"key":26,"text":27,"correct":14},"E","取5个试块抗压强度的平均值作为砂浆的强度值","BD","2020\u002F2019版教材P50 将砂浆做成70.7mm×70.7mm×70.7mm的立方体试块，标准养护28天（温度20±2℃，相对湿度90%以上），每组取3个试件进行抗压强度试验。",{"id":6,"name":31,"category":32,"favorite":33},"一建建筑工程实务","建筑工程",0]