[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1143630":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1143630,800,2,"多选题","关于混凝土工程冬期施工的说法， 正确的有（）。",[11,15,19,22,25],{"key":12,"text":13,"correct":14},"A","可加热矿物掺合料以满足热工计算要求",false,{"key":16,"text":17,"correct":18},"B","预拌混凝土或远距离输送的混凝土，拌合物的出机温度不宜低于15℃",true,{"key":20,"text":21,"correct":18},"C","混凝土入模温度不应低于5℃",{"key":23,"text":24,"correct":14},"D","在混凝土养护和越冬期间，可以采用浇水养护",{"key":26,"text":27,"correct":18},"E","应增设2组与结构同条件养护试件","BCE","冬期（连续 5 天最低温度低于 5℃）混凝土施工要点： （1）冬期施工混凝土搅拌时间应比常温搅拌时间延长 30~60s。 （2）应优先采用加热水的方法，严禁加热水泥、掺合料或外加剂。 （3）预拌混凝土和远距离运输混凝土拌合物出机温度不宜低于 15℃，混凝土入模温度不应低于5℃。 （4）分层浇筑时， 分层厚度不应小于 400mm；且上层混凝土覆盖前， 已浇筑混凝土温度不得低于 2℃（防止前层混凝土冻融）。",{"id":6,"name":31,"category":32,"favorite":33},"一建建筑工程实务","建筑工程",0]