[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1143349":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},1143349,799,1,"单选题","（2019年真题）某混凝土结构岀现宽度为0.5mm的裂缝且裂缝深度较深，应采用的处理方法是（）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","灌浆修补法",true,{"key":16,"text":17,"correct":18},"B","表面密封法",false,{"key":20,"text":21,"correct":18},"C","嵌缝封闭法",{"key":23,"text":24,"correct":18},"D","粘钢加固法","P191-194 对混凝上结构出现裂缝,经分析研究后如果不影响结构的安全和使用功时,也可采取返修处理。当裂缝宽度不大于0.2mm时,可采用表面密封法;当裂宽度大于0.3mm时,采用嵌缝密闭法;当裂缝较深时,则应采取灌浆修补的方法。本题中裂缝宽度较深,所以采取灌浆修补法。",{"id":6,"name":27,"category":28,"favorite":29},"一建建设工程项目管理","建筑工程",0]