[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1136602":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},1136602,797,1,"单选题","（2018年真题）不符合耐火陶瓷纤维施工技术要求的是（ ）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","制品不得受挤压",false,{"key":16,"text":17,"correct":18},"B","制品粘贴时不受潮湿影响",true,{"key":20,"text":21,"correct":14},"C","粘贴面应清洁和平整",{"key":23,"text":24,"correct":14},"D","粘结剂使用时应搅拌均匀","耐火陶瓷纤维施工技术要求一般规定 （1）制品的技术指标和结构形式符合设计要求； （2）制品不得受潮和挤压； （3）切割制品时，其切口应整齐； （4）粘结剂使用时应搅拌均匀； （5）粘贴面应清洁、干燥、平整，粘切面应均匀涂刷粘结剂； （6）制品表面涂刷耐火涂料时，涂料应均匀、满布，多层涂刷时，前后层应交错； （7）在耐火陶瓷纤维内衬上施工不定形耐火材料时，其表面应做防水处理。",{"id":6,"name":27,"category":28,"favorite":29},"一建机电工程实务","建筑工程",0]