[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1130560":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},1130560,794,2,"多选题","对于混凝土拌合物运送至浇筑地点时出现离析、分层或稠度不满足要求的处理，正确的方法有（ ）。",[11,15,19,22,25],{"key":12,"text":13,"correct":14},"A","对混凝土拌合物进行二次搅拌",true,{"key":16,"text":17,"correct":18},"B","少量加水二次搅拌",false,{"key":20,"text":21,"correct":14},"C","加入水和胶凝材料搅拌",{"key":23,"text":24,"correct":14},"D","保持水胶比不变",{"key":26,"text":27,"correct":18},"E","直接废弃","ACD","2020版教材页码P106-P108 混凝土拌合物运送至浇筑地点如出现离析、分层或稠度不满足要求等现象，应对混凝土拌合物进行二次搅拌。二次搅拌时不得任意加水。稠度不足时可同时加入水和胶凝材料，保持其水胶比不变。采用泵送混凝土时供应的混凝土量应能保证混凝土泵的连续工作。如因故间歇，间歇时间不应超过45min。",{"id":6,"name":31,"category":32,"favorite":33},"一建港口与航道工程实务","建筑工程",0]