[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1126129":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":19,"analysis":25},1126129,792,1,"单选题","（2012年真题）在常温条件下，水泥稳定土基层的养护时间至少应（ ）天。",[11,15,18,22],{"key":12,"text":13,"correct":14},"A","5",false,{"key":16,"text":17,"correct":14},"B","6",{"key":19,"text":20,"correct":21},"C","7",true,{"key":23,"text":24,"correct":14},"D","8","本题考查的是不同基层施工技术要求。水泥稳定土基层必须保湿养护，防止忽干忽湿，常温下成活后应经7d养护，方可在其上铺筑上层。",{"id":6,"name":27,"category":28,"favorite":29},"二建市政工程实务","建筑工程",0]