[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1125677":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},1125677,792,1,"单选题","粗集料为主的热拌沥青混合料复压采用振动压路机，相邻碾压带宜重叠（）cm。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","10～20",true,{"key":16,"text":17,"correct":18},"B","20～30",false,{"key":20,"text":21,"correct":18},"C","30～40",{"key":23,"text":24,"correct":18},"D","40～50","P19-22 对粗集料为主的混合料，宜优先采用振动压路机复压(厚度宜大于30mm)，振动频率宜为35~50Hz，振幅宜为0.3~0.8mm。层厚较大时宜采用高频大振幅，厚度较薄时宜采用低振幅，以防止集料破碎。相邻碾压带宜重叠100~200mm。",{"id":6,"name":27,"category":28,"favorite":29},"二建市政工程实务","建筑工程",0]