[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1125052":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},1125052,792,1,"单选题","在混凝土生产过程中，对骨料含水率的检测，每一工作班不应少于( )次。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","1",true,{"key":16,"text":17,"correct":18},"B","2",false,{"key":20,"text":21,"correct":18},"C","3",{"key":23,"text":24,"correct":18},"D","4","2021\u002F2020版教材P40页 在混凝土生产过程中，应注意控制原材料的计量偏差。对骨料的含水率的检测，每工作班不应少于一次，雨期施工应增加测定次数。",{"id":6,"name":27,"category":28,"favorite":29},"二建市政工程实务","建筑工程",0]