[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1124501":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":19,"analysis":25},1124501,792,1,"单选题","关于预应力混凝土配制的说法错误的是（ ）。",[11,15,18,22],{"key":12,"text":13,"correct":14},"A","预应力混凝土应优先采用硅酸盐水泥、普通硅酸盐水泥，不宜使用矿渣硅酸盐水泥，不得使用火山灰质硅酸盐水泥及粉煤灰硅酸盐水泥",false,{"key":16,"text":17,"correct":14},"B","粗骨料应采用碎石，其粒径宜为5-25mm",{"key":19,"text":20,"correct":21},"C","混凝土中的水泥用量宜大于550kg\u002Fm2",true,{"key":23,"text":24,"correct":14},"D","从各种材料引入混凝土中的氯离子总含量（折合氯化物含量）不宜超过水泥用量的0.06%","预应力混凝土的配制要求如下所述。(1)预应力混凝土应优先采用硅酸盐水泥，普通硅酸盐水泥，不宜使用矿渣硅酸盐水泥，不得使用火山灰质硅酸盐水泥及粉煤灰硅酸盐水泥。粗骨料应采用碎石，其粒径宜为5-25mm。(2)混凝土中的水泥用量不宜大于550kg\u002Fm3。(3)混凝土中严禁使用含氯化物的外加剂及引气剂或引气型减水剂。(4)从各种材料引入混凝土中的氯离子总含量（折合氯化物含量）不宜超过水泥用量的0.06%。超过0.06%时，宜采取掺加阻锈剂、增加保护层厚度、提高混凝土密实度等防锈措施。",{"id":6,"name":27,"category":28,"favorite":29},"二建市政工程实务","建筑工程",0]