[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-1120350":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},1120350,790,1,"单选题","防水混凝土试配时的抗渗等级应比设计要求提高（）MPa。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","0.1",false,{"key":16,"text":17,"correct":18},"B","0.2",true,{"key":20,"text":21,"correct":14},"C","0.3",{"key":23,"text":24,"correct":14},"D","0.4","防水混凝土可通过调整配合比，或掺加外加剂、掺合料等措施配制而成，其抗渗等级不得小于P6，其试配混凝土的抗渗等级应比设计要求提高0.2MPa。",{"id":6,"name":27,"category":28,"favorite":29},"二建建筑工程实务","建筑工程",0]