[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-979266":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},979266,707,1,"单选题","检查混凝土设计强度等级的试块应如何养护？",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","20&deg;C&plusmn;2&deg; C，95%相对湿度下养护28d",true,{"key":16,"text":17,"correct":18},"B","15&deg;C&plusmn;3&deg; C，80%相对湿度下养护28d",false,{"key":20,"text":21,"correct":18},"C","25&deg;C&plusmn;3&deg;90%相对湿度下养护28d",{"key":23,"text":24,"correct":18},"D","25&deg;C&plusmn;3&deg;90%相对湿度下养护7d","提示：为了评定结构构件的混凝土强度等级，应采用标准试件的混凝土强度，即边长150mm的标准试块，在温度为20&deg;C&plusmn;2&deg;C，相对湿度为95%的标准条件下，养护至28d龄期时的实测抗压强度。 .",{"id":6,"name":27,"category":28,"favorite":29},"岩土专业基础知识","建筑工程",0]