[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-904780":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},904780,585,1,"单选题","关于固结灌浆施工技术要求，下列说法错误的是（ ）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","灌浆孔灌浆前的压水试验孔数不宜少于总孔数的5%",false,{"key":16,"text":17,"correct":18},"B","固结灌浆质量压水试验检查应在灌浆结束14d后进行",true,{"key":20,"text":21,"correct":14},"C","灌浆孔应采用压力水进行裂隙冲洗，冲洗压力值不超过1MPa",{"key":23,"text":24,"correct":14},"D","灌浆孔封孔可采用“压力灌浆封孔法”","A项，在固结灌浆施工工艺中，灌浆孔灌浆前的压水试验应在裂隙冲洗后进行，采用单点法。压水试验孔数不宜少于总孔数的5%。B项，固结灌浆质量压水试验检查、岩体波速检查、静弹性模量检查应分别在灌浆结束3～7d、14d、28d后进行。C项，灌浆孔应采用压力水进行裂隙冲洗，直至回水清净时止。冲洗压力可为灌浆压力的80%，该值若大于1MPa时，采用1MPa。D项，灌浆孔封孔应采用“机械压浆封孔法”或“压力灌浆封孔法”。",{"id":6,"name":27,"category":28,"favorite":29},"建设工程技术与计量（水利）","建筑工程",0]