[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-903929":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},903929,584,2,"多选题","下列关于热拌沥青混合料路面的施工工艺说法正确的有（ ）。",[11,15,18,22,25],{"key":12,"text":13,"correct":14},"A","表面温度低于50℃后方可开放交通",true,{"key":16,"text":17,"correct":14},"B","沥青的加热温度控制在150～170℃",{"key":19,"text":20,"correct":21},"C","低于规定铺筑温度混合料应二次加热后使用",false,{"key":23,"text":24,"correct":21},"D","出现离析、边角缺料等现象时应减小摊铺机速度",{"key":26,"text":27,"correct":14},"E","采用雾状喷水法，可保证沥青混合料碾压过程中不粘轮","ABE","A项，热拌热铺沥青混合料路面应待摊铺层完全自然冷却，表面温度低于50℃后方可开放交通。一般在施工完毕后第二天可开放交通；B项，沥青的加热温度控制在150～170℃。集料的加热温度控制在160～180℃，混合料的出厂温度控制在140～165℃，混合料运至施工现场的温度控制在120～150℃；C项，已经离析或结成团块或卸料时滞留于车上的混合料，以及低于规定铺筑温度或被雨水淋湿的混合料都应废弃；D项，出现离析、边角缺料等现象时人工及时补撒料，换补料，摊铺过程中不准随意变换速度或中途停顿；E项，压实时采用雾状喷水法，以保证沥青混合料碾压过程中不粘轮。",{"id":6,"name":31,"category":32,"favorite":33},"建设工程技术与计量（交通）","建筑工程",0]