[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-903344":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},903344,584,1,"单选题","混凝土抗压强度应以边长150mm的立方体标准试件测定，保证率95%，试件以同龄期3个为一组，每组试件抗压强度以3个试件测值的算术平均值为测定值（精确至0.1MPa），当有1个测值与中间值的差值超中间值15%时（ ）",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","该组试验无效",false,{"key":16,"text":17,"correct":18},"B","取中间值为测定值",true,{"key":20,"text":21,"correct":14},"C","取最小值为测定值",{"key":23,"text":24,"correct":14},"D","取平均值为测定值","混凝土抗压强度应以边长150mm的立方体标准试件测定，保证率95%，试件以同龄期3个为一组，每组试件抗压强度以3个试件测值的算术平均值为测定值（精确至0.1MPa），当有1个测值与中间值的差值超中间值15%时取中间值为测定值，当有2个测值与中间值的差值均超15%时则该组试验无效。混凝土抗压强度应以标准方式成型的试件置于标准养护条件下（温度20℃±2℃，相对温度不低于95%）养护28天所测得的抗压强度值（MPa）进行测定。",{"id":6,"name":27,"category":28,"favorite":29},"建设工程技术与计量（交通）","建筑工程",0]