[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-900851":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":25},900851,583,1,"单选题","某焊接方法，热效率高、熔深大、焊接速度快、机械化操作程度高，因而适用于中厚板结构平焊位置长焊缝的焊接，该焊接方法是（ ）。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","埋弧焊",true,{"key":16,"text":17,"correct":18},"B","钨极惰性气体保护焊",false,{"key":20,"text":21,"correct":18},"C","熔化极气体保护焊",{"key":23,"text":24,"correct":18},"D","等离子弧焊","2020版教材P72 P68-69 埋弧焊的主要优点是：热效率较高，熔深大，工件的坡口可较小，减少了填充金属量；焊接速度高，当焊接厚度为8~10mm的钢板时，单丝埋弧焊速度可达50-80cm\u002Fmin；焊剂的存在不仅能隔开熔化金属与空气的接触，而且使熔池金属较慢地凝固，减少了焊缝中产生气孔、裂纹等缺陷的可能性。但由于采用颗粒状焊剂，这种焊接方法一般只适用于平焊位置，且不能直接观察电弧与坡口的相对位置，容易焊偏。另外，不适于焊接厚度小于1mm的薄板。由于埋弧焊熔深大，生产效率高，机械化操作的程度高，因而适于焊接中厚板结构的长焊缝和大直径圆通的环焊缝。",{"id":6,"name":27,"category":28,"favorite":29},"建设工程技术与计量（安装)","建筑工程",0]