[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-900842":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":22,"analysis":25},900842,583,1,"单选题","将钢件加热到临界点Ac3（对亚共析钢而言，是指珠光体全部转变为奥氏体，过剩相铁素体也完全消失的温度）以上的适当温度，在炉内保温缓慢冷却的热处理工艺为（ ）。",[11,15,18,21],{"key":12,"text":13,"correct":14},"A","去应力退火",false,{"key":16,"text":17,"correct":14},"B","球化退火",{"key":19,"text":20,"correct":14},"C","不完全退火",{"key":22,"text":23,"correct":24},"D","完全退火",true,"2020版教材P83 焊后热处理的特点，“完全退火是将钢件加热到临界点Ac3（对亚共析钢而言，是指珠光体全部转变为奥氏体、过剩相铁素体也完全消失的温度）以上的适当温度，在炉内保温缓慢冷却的工艺方法。其目的是细化组织、降低硬度、改善加工性能去除内应力。完全退火适用于中碳钢和中碳合金钢的铸、焊、轧制件等。”",{"id":6,"name":27,"category":28,"favorite":29},"建设工程技术与计量（安装)","建筑工程",0]