[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-900840":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":22,"analysis":25},900840,583,1,"单选题","它不属于熔化极电弧焊，适用于薄板及超薄板的焊接，其功率密度比自由电弧提高100倍以上，焊接速度快、生产效率高，穿透力强，但设备比较复杂，工艺参数调节匹配较复杂。该焊接方式为（ ）。",[11,15,18,21],{"key":12,"text":13,"correct":14},"A","电渣压力焊",false,{"key":16,"text":17,"correct":14},"B","氩弧焊",{"key":19,"text":20,"correct":14},"C","钨极惰性气体保护焊",{"key":22,"text":23,"correct":24},"D","等离子弧焊",true,"2020版教材P74 等离子弧焊接的特点，“等离子弧焊是自由电弧压缩而成的，其功率密度比自由电弧可提高100倍以上。等离子弧焊与钨极惰性气体保护焊相比有以下特点：1）等离子弧能量集中、温度高，焊接速度快，生产率高。2）穿透能力强，对于大多数金属在一定厚度范围内都能获得锁孔效应，可一次行程完成8mm以下直边对接接头单面焊双面成型的焊缝。焊缝致密，成形美观。3）电弧挺直度和方向性好，可焊接薄壁结构（如1mm以下金属箔的焊接）。4）设备比较复杂、气体耗量大，费用较高，只宜于室内焊接。",{"id":6,"name":27,"category":28,"favorite":29},"建设工程技术与计量（安装)","建筑工程",0]