[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-894456":3},{"question":4,"library":30},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":28,"analysis":29},894456,580,2,"多选题","防水混凝土施工应满足的工艺要求有（ ）。",[11,15,18,21,25],{"key":12,"text":13,"correct":14},"A","保持施工环境干燥，避免带水施工",true,{"key":16,"text":17,"correct":14},"B","防水混凝土应自然养护，养护时间不少于14d",{"key":19,"text":20,"correct":14},"C","防水混凝土采用预拌混凝土时，入泵坍落度宜控制在120～140mm",{"key":22,"text":23,"correct":24},"D","混凝土中不宜掺和膨胀水泥",false,{"key":26,"text":27,"correct":14},"E","喷射混凝土终凝2h后应采取喷水养护，养护时间不得少于14d","ABCE","防水混凝土在施工中应注意的事项：①保持施工环境干燥，避免带水施工。②防水混凝土采用预拌混凝土时，入泵坍落度宜控制在120～140mm，坍落度每小时损失不应大于20mm，坍落度总损失值不应大于40mm。③防水混凝土浇筑时的自落高度不得大于1.5m；防水混凝土应采用机械振捣，并保证振捣密实。④防水混凝土应自然养护，养护时间不少于14d。⑤喷射混凝土终凝2h后应采取喷水养护，养护时间不得少于14d；当气温低于5℃时，不得喷水养护。⑥防水混凝土结构的变形缝、施工缝、后浇带、穿墙管、埋设件等设置和构造必须符合设计要求。D项，常用的防水混凝土有普通防水混凝土、外加剂或掺和料防水混凝土和膨胀水泥防水混凝土。",{"id":6,"name":31,"category":32,"favorite":33},"[土木建筑工程]建设工程计量与计价实务","建筑工程",0]