[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-776430":3},{"question":4,"library":26},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":16,"analysis":25},776430,441,1,"单选题","低氢焊条一般在常温下超过（），应重新烘干。",[11,15,19,22],{"key":12,"text":13,"correct":14},"A","2h",false,{"key":16,"text":17,"correct":18},"B","4h",true,{"key":20,"text":21,"correct":14},"C","8h",{"key":23,"text":24,"correct":14},"D","10h","",{"id":6,"name":27,"category":28,"favorite":29},"承压焊","特种作业",0]