[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-724035":3},{"question":4,"library":23},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":22},724035,406,1,"单选题","等离子弧焊焊接速度比钨极氩弧焊()。",[11,15,19],{"key":12,"text":13,"correct":14},"A","快",true,{"key":16,"text":17,"correct":18},"B","相当",false,{"key":20,"text":21,"correct":18},"C","慢","等离子弧焊的焊缝成形具有深而窄的特点，热影响小，等离子弧焊缝深而窄，典型的酒杯状焊缝，几乎显示不出热影响区；而钨极氩弧焊的热影响区达到3~4mm，适于焊接对热作用较敏感的钢材，例如奥氏体不锈钢和耐热钢等。因此等离子弧焊具有焊接速度快；焊缝深度比大，截面积小；薄板焊接变形小，厚板焊接缩孔倾向小及热影响区窄等特点。",{"id":6,"name":24,"category":25,"favorite":26},"熔化焊接与热切割","特种作业",0]