[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-723652":3},{"question":4,"library":23},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":22},723652,406,1,"单选题","为提高钢铁材料的弹性极限和屈服强度,同时保证较好的韧性,最好采用()。",[11,15,19],{"key":12,"text":13,"correct":14},"A","中温回火",true,{"key":16,"text":17,"correct":18},"B","低温回火",false,{"key":20,"text":21,"correct":18},"C","高温回火","低温回火（加热温度通常为150℃～250℃）可减小工件的淬火应力、降低脆性并保持高硬度。用于要求硬度高、耐磨性好的零件，如刀具、模具等。 中温回火（加热温度为350C～500℃）可显著减小淬火应力，提高弹性。常用于各种弹簧和某些模具。 高温回火（加热温度为500℃～650℃）可消除淬火应力，使零件获得优良的综合力学性能。通常把“淬火加高温回火”称为调质。调质广泛用于处理各种重要的中碳钢零件，尤其是承受动载荷的零件，如各种轴、齿轮等。",{"id":6,"name":24,"category":25,"favorite":26},"熔化焊接与热切割","特种作业",0]