[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-723650":3},{"question":4,"library":23},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":12,"analysis":22},723650,406,1,"单选题","为便于引弧和提高电弧稳定性,直流正接的等离子弧焊工艺中,电极端部应磨成()。",[11,15,19],{"key":12,"text":13,"correct":14},"A","20°至60°的夹角",true,{"key":16,"text":17,"correct":18},"B","\u003C10°的夹角",false,{"key":20,"text":21,"correct":18},"C","70°至80°的夹角","等离子弧钨极特点： (1) 材料:等离子弧电极材质与氩弧电极材质相同，国内主要采用钍钨极、铈钨极，国外还采用锆钨极。 (2) 形状:指钨极端部要求的形状，为便于引弧和提高电弧稳定性，将钨极端部磨成20°〜60°夹角的尖状或呈圆台形、大电流时磨成圆台尖锥形。 (3) 许用电流:钨极直径固定后，允许使用的最大电流。",{"id":6,"name":24,"category":25,"favorite":26},"熔化焊接与热切割","特种作业",0]