[{"data":1,"prerenderedAt":-1},["ShallowReactive",2],{"q-671605":3},{"question":4,"library":20},{"id":5,"libraryId":6,"type":7,"typeLabel":8,"stem":9,"options":10,"answer":17,"analysis":19},671605,384,3,"判断题","采用E310-15焊条焊接1Cr18Ni9不锈钢和Q235低碳钢，如熔合比为40%时，则焊缝为抗裂性能较高的奥氏体+铁素体组织。",[11,15],{"key":12,"text":13,"correct":14},"A","正确",false,{"key":16,"text":17,"correct":18},"B","错误",true,"",{"id":6,"name":21,"category":22,"favorite":23},"焊工（技师）","技能鉴定",0]